Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 553 g/mol | 553 g/mol | |
Oceanchem Group Antioxidant 1024 Molecular Formula: C34H52N2O4Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of b.. |