Material Notes:
Molecular Formula: C34H52N2O4Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of bak, wire and cable.Storage and Packing: Stored in a dark and dry place in room temperature, plastic bag lined carton.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Molecular Weight 553 g/mol
553 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 224 - 229 °C
435 - 444 °F
Optical Properties Metric English Comments
Transmission, Visible 96 %

@Wavelength 425 nm
96 %

@Wavelength 425 nm
toluene solution
98 %

@Wavelength 500 nm
98 %

@Wavelength 500 nm
toluene solution
Descriptive Properties Value Comments
Appearance White crystalline powder
Assay (%) >99
Molecular Formula C34H52N2O4
Solubility 0.1
toluene (25°C, Wt)
Users viewing this material also viewed the following: