Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 8000 g/mol | 8000 g/mol | |
Solvay Specialty Polymers FOMBLIN® M15 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Molecular Weight | 8000 g/mol | 8000 g/mol | |
Solvay Specialty Polymers FOMBLIN® Z15 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |
|||
Molecular Weight | 8000 g/mol | 8000 g/mol | |
Unitika elitel UE3380 Polyester, Flake Low molecular weight type UE3200, Low softening point, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products.. |