Material Notes:
Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
ASTM D891
Viscosity Measurement 286
286
Viscosity Index; ASTM D2270
Kinematic Viscosity 150 cSt

@Temperature 20.0 °C
150 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 85 cSt
85 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 22 cSt
22 cSt
ASTM D445
Molecular Weight 8000 g/mol
8000 g/mol
Evaporation Loss 0.80 %
0.80 %
22 hrs. at 149°C; ASTM 2595
3.0 %
3.0 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 24 dynes/cm
24 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 114 kg
251 lb (mass)
Mean Hertz Load; IP 239
398 kg
878 lb (mass)
Init. Seiz. Load; IP 239
562 kg
1240 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.920 mm

@Load 40.0 kg,
Temperature 75.0 °C
0.0362 in

@Load 88.2 lb,
Temperature 167 °F
Avg. scar diameter; 1200 RPM, 60 min; ASTM D4172 B
Thermal Properties Metric English Comments
Pour Point -75.0 °C
-103 °F
ASTM D97