Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Base Resin Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |