Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.500 - 50.0 g/10 min @Temperature 230 - 230 °C |
0.500 - 50.0 g/10 min @Temperature 446 - 446 °F |
Average value: 15.1 g/10 min Grade Count:17 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Base Resin Melt Index | 0.500 - 25.0 g/10 min | 0.500 - 25.0 g/10 min | Average value: 6.32 g/10 min Grade Count:9 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |