Polymer Property : Base Resin Melt Index = 50.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 0.500 - 50.0 g/10 min

@Temperature 230 - 230 °C
0.500 - 50.0 g/10 min

@Temperature 446 - 446 °F
Average value: 15.1 g/10 min Grade Count:17
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..