Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | >= 1000 hour | >= 1000 hour | ASTM D2561 |
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 818-073 offers the high environmental stress crack resistance characteristics of linear low density polyethylene with the processing properties needed for blowmolding and e.. |
|||
ESCR, Bottle | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LP5002 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LP series of polyethylene resins exhibits excellent environmental stress crack resistance and is especially designed for bottles containing aggressive agricultural and hou.. |
|||
ESCR, Bottle | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
ESCR, Bottle | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
ESCR, Bottle | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |