Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | >= 50 hour @Temperature 23.0 °C |
>= 50 hour @Temperature 73.4 °F |
F<sub>50</sub>; ASTM D1693 |
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding Applications:Large dustbins and pailsPallet boxesFish cratesTechnical moldingInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |