Polymer Property : Environmental Stress Crack Resistance = 5000 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance >= 5000 hour

@Temperature 100 °C
>= 5000 hour

@Temperature 212 °F
F<sub>50</sub> Cond. C; ASTM D 1693
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Characteristics: PPI Recommended Hydrostatic Design Bases (HDB): 1250..
Environmental Stress Crack Resistance >= 5000 hour

@Temperature 100 °C
>= 5000 hour

@Temperature 212 °F
F<sub>50</sub> Cond. C; ASTM D 1693
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe..
Environmental Stress Crack Resistance >= 5000 hour

@Temperature 100 °C
>= 5000 hour

@Temperature 212 °F
F<sub>50</sub> Cond. C; ASTM D 1693
Chevron Phillips HiD® 9302 HDPE Yellow Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Applications:Natural Gas Distribution Piping and FittingsData provide..