Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Characteristics: PPI Recommended Hydrostatic Design Bases (HDB): 1250 psi at 73°F, 1000 psi at 140°FApplications:Natural Gas Distribution Piping and FittingsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 2000 hour

@Temperature 50.0 °C
>= 2000 hour

@Temperature 122 °F
F<sub>50</sub>, Cond. B.; ASTM D1693
>= 5000 hour

@Temperature 100 °C
>= 5000 hour

@Temperature 212 °F
F<sub>50</sub> Cond. C; ASTM D 1693
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Stiffness Modulus 0.790 GPa
115 ksi
3 pt. secant ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -59.0 °C
<= -74.2 °F
ASTM D746