Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Permeability | 0.590 g mil/ (m2 day) @Temperature 37.0 °C |
0.0381 g mil/ (100 in2 day) @Temperature 98.6 °F |
90% RH; ASTM E96 |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |