Physical Properties Metric English Comments
ESCR 10% Igepal® >= 15000 hour

@Temperature 50.0 °C
>= 15000 hour

@Temperature 122 °F
No Failure after 15,000 hours; Igepal CO630; ASTM D1693
LyondellBasell Montell 0300 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive..
ESCR 10% Igepal® >= 15000 hour

@Temperature 50.0 °C
>= 15000 hour

@Temperature 122 °F
No Failure after 15,000 hours; Igepal CO630; ASTM D1693
LyondellBasell Montell 0800 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe..
ESCR 10% Igepal® >= 15000 hour

@Temperature 50.0 °C
>= 15000 hour

@Temperature 122 °F
No Failure after 15,000 hours; Igepal CO630; ASTM D1693
LyondellBasell DP 0110M Polybutene
Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i..