Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F<SUB>50</SUB>; CO-630; ASTM D1693 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | molding; ASTM D1693 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Thickness 1.90 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.0748 in, Temperature 122 °F |
slit; ASTM D1693 |
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Alathon® L5040TC High Density Polyethylene ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693-01 |
Ipiranga Petrochem GP 100 BK HDPE The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693-01 |
Ipiranga Petrochem GP 100 OR HDPE The resin GP 100 OR is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |