Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000300 - 0.0200 cm/cm | 0.000300 - 0.0200 in/in | Average value: 0.00890 cm/cm Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0100 cm/cm | 0.000300 - 0.0100 in/in | Average value: 0.00539 cm/cm Grade Count:11 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0150 cm/cm | 0.000300 - 0.0150 in/in | Average value: 0.00402 cm/cm Grade Count:139 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00391 cm/cm Grade Count:183 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0200 cm/cm | 0.000300 - 0.0200 in/in | Average value: 0.00496 cm/cm Grade Count:111 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00417 cm/cm Grade Count:497 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.00700 cm/cm | 0.000300 - 0.00700 in/in | Average value: 0.00163 cm/cm Grade Count:32 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00325 cm/cm Grade Count:111 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.00780 cm/cm | 0.000300 - 0.00780 in/in | Average value: 0.00304 cm/cm Grade Count:17 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |