Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00600 - 0.0100 cm/cm | 0.00600 - 0.0100 in/in | ASTM D955 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.000300 - 0.0100 cm/cm | 0.000300 - 0.0100 in/in | Average value: 0.00539 cm/cm Grade Count:11 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00599 cm/cm Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00443 cm/cm Grade Count:20 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00514 cm/cm Grade Count:131 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.000700 - 0.0100 cm/cm | 0.000700 - 0.0100 in/in | Average value: 0.00319 cm/cm Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0100 cm/cm | 0.00400 - 0.0100 in/in | Average value: 0.00636 cm/cm Grade Count:21 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00502 cm/cm Grade Count:90 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00164 cm/cm Grade Count:50 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00514 cm/cm Grade Count:11 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00531 cm/cm Grade Count:104 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.0100 cm/cm | 0.000200 - 0.0100 in/in | Average value: 0.00308 cm/cm Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00342 cm/cm Grade Count:26 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00356 cm/cm Grade Count:76 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00250 - 0.0100 cm/cm | 0.00250 - 0.0100 in/in | Average value: 0.00541 cm/cm Grade Count:13 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00833 cm/cm Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00525 cm/cm Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00624 cm/cm Grade Count:373 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0100 cm/cm | 0.000100 - 0.0100 in/in | Average value: 0.00414 cm/cm Grade Count:227 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00429 cm/cm Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00385 cm/cm Grade Count:79 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00374 cm/cm Grade Count:45 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00311 cm/cm Grade Count:14 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00180 - 0.0100 cm/cm | 0.00180 - 0.0100 in/in | Average value: 0.00549 cm/cm Grade Count:14 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.000800 - 0.0100 cm/cm | 0.000800 - 0.0100 in/in | Average value: 0.00627 cm/cm Grade Count:9 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |