Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0023 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ISO 294-4
PolyOne Edgetek® NJ-30GF/000 natural Polyamide 12 (Nylon 12)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced
Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d..
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ISO 2577
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic
Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by ..
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac
FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at..
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0023 cm/cm
0.0023 in/in
ASTM D955
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Copyright © lookpolymers.com All Rights Reserved