Polymer Property : Linear Mold Shrinkage = 0.0036 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0024 - 0.0036 cm/cm
0.0024 - 0.0036 in/in
IS 13411-1992
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..