Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0024 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0024 - 0.0030 in/in

@Thickness 0.125 in
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced
Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All ..
Linear Mold Shrinkage 0.0024 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0024 - 0.0030 in/in

@Thickness 0.125 in
Ovation Polymers OPTRENE 30GF Polypropylene, 30% Glass Reinforced
Properties of chemically coupled glass reinforced (30%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All ..
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
ASTM D955-89
Multibase Multi-ABS 8933 Black
Ash is 28% per ASTM D-5630-94.Data provided by Multibase.
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
Bayer Test
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C..
Linear Mold Shrinkage 0.0024 - 0.0036 cm/cm
0.0024 - 0.0036 in/in
IS 13411-1992
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
ATM D955
Plenco 50335 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform..