Polymer Property : Linear Mold Shrinkage = 0.0052 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
Multibase Multi-Flex® TPE A 7699 BLK
Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural
Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black
Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
STN 64 0808
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
STN 64 0808
Plastcom SLOVAMID 66 GF 25 FRI 3 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder
FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with ..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
STN 64 0808
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling
FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi..
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
Plenco 1508 Polyester, Briquette, Injection Molded
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl..
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
Plenco 4548 Phenolic, Granular, Transfer Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.