Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 6 GF 30 002 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used for holders of hand tools, hobby tools, gear wheel.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 6 GF 30 031 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized, better surface appearance of injection moldings. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used f.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | |
Plastcom SLOVALEN PC 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. A.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, .. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | STN EN ISO 294-4 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | per ATM D955. Post shrinkage is 0.15% at 72hr 120ºC per ASTM D1299. |
Plenco 7466 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Linear Mold Shrinkage | 0.0058 - 0.0080 cm/cm | 0.0058 - 0.0080 in/in | ASTM D955 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | ASTM D955 |
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | ASTM D955 |
Plenco 7476 Phenolic, Granular, Transfer Molded PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. .. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | |
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Linear Mold Shrinkage | 0.0058 cm/cm | 0.0058 in/in | ASTM D955 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |