Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | |
Plastcom SLOVALEN PH 69 GF 20 T 10 PP, 20% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre and 10 % Talc, contains themodifier of mechanical properties.Increased strength in comparison with .. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | per ATM D955. Post shrinkage is 0.23% at 72hr 120ºC per ASTM D1299. |
Plenco 4224 Phenolic, Granular, Transfer Molded
(discontinued **) Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b.. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | Isotropy |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Linear Mold Shrinkage | 0.0062 cm/cm | 0.0062 in/in | ASTM D955 |
Teknor Apex Sinpolene GPP1610 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 10% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |