Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
STN EN ISO 294-4
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber
PA66 reinforced with 20 % glass fiber, used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear w..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
STN 64 0808
Plastcom SLOVAMID 66 CF 20 Polyamide 66, 20% Carbon Fiber
FeaturesChemically reinforced with 20% carbon fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. ..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
Plastcom SLOVAMID 66 GF 20 PA66, 20% glass fibre
FeaturesChemically reinforced with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. ..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
Plastcom SLOVAMID 66/6 GF 20 PA66/6, 20% glass fibre
FeaturesChemically reinforced alloy PA 66 and PA 6 with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and ..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12  (discontinued **)
Information provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Plenco 1500 Polyester, Granular, Transfer Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Plenco 2571 Phenolic, Granular, Transfer Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Plenco 7523 Phenolic, Granular, Transfer Molded
PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P..