Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Aramid Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
Mechanical Properties Metric English Comments
Tensile Stress 85.0 MPa
12300 psi
Elongation at Yield 6.0 %
6.0 %
8.0 %
8.0 %
flexural
Modulus of Elasticity 4.00 GPa
580 ksi
Flexural Strength 120 MPa
17400 psi
Flexural Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.16
0.16
Coefficient of Friction, Static 0.14
0.14
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Vicat Softening Point 260 °C
500 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color green beige