Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0156 cm/cm
0.0156 in/in
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh..