Material Notes:
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased shrinkage. General application in all industry branches - packing material, garden flower-pots, toys, furniture industry, dowels, clamps, hinge, office chairs, hangers, covers of car chassis, fenders, motors etc. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage 0.0156 cm/cm
0.0156 in/in
Linear Mold Shrinkage, Transverse 0.0135 cm/cm
0.0135 in/in
Melt Flow 12 g/10 min

@Load 0.325 kg,
Temperature 270 °C
12 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 MPa
4640 psi
Elongation at Break 6.0 %
6.0 %
Tensile Modulus 2.40 GPa
348 ksi
Flexural Strength 46.0 MPa
6670 psi
Flexural Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Vicat Softening Point 160 °C
320 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi