Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0181 cm/cm | 0.0181 in/in | |
Plastcom SLOVALEN PH 91 N PP, basic type FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered.. |
|||
Linear Mold Shrinkage | 0.0181 cm/cm @Thickness 4.00 mm |
0.0181 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |