Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0200 - 0.0500 cm/cm | 0.0200 - 0.0500 in/in | Average value: 0.0318 cm/cm Grade Count:28 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.0200 - 0.0450 cm/cm | 0.0200 - 0.0450 in/in | Average value: 0.0272 cm/cm Grade Count:12 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Linear Mold Shrinkage | 0.0200 - 0.0600 cm/cm | 0.0200 - 0.0600 in/in | Average value: 0.0386 cm/cm Grade Count:7 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |