Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/20T Polyester (PBT) - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Kolon KOCETAL® K100 Standard Grade Acetal Resin Suitable for extrusion and injection molding of thick products. Applications: Extruded use such as rod, pipe, tube, and sheetInformation provided by API Kolon. |
|||
Linear Mold Shrinkage | 0.022 - 0.027 cm/cm | 0.022 - 0.027 in/in | ASTM D955 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break AAROLENE® ARPP 200-4 Series Polypropylene Compounded ResinFeatures: A copolymer polypropylene resin, pre-colored black, featuring excellent toughness for all extrusion applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A pre-colored, black homopolymer polypropylene resin specifically designed for all injection molding applications.High Flow |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.022 - 0.024 cm/cm | 0.022 - 0.024 in/in | ASTM D955 |
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone
(discontinued **) Information provided by PolyOne™ Corporation |