Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name LIMS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Viscosity 400000 cP
400000 cP
A
400000 cP
400000 cP
B
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength 9.20 MPa
1330 psi
Elongation at Yield 600 %
600 %
100% Modulus 0.00109 GPa
0.158 ksi
Tear Strength 42.0 kN/m
240 pli
Compression Set 5.0 %

@Temperature 200 °C,
Time 14400 sec
5.0 %

@Temperature 392 °F,
Time 4.00 hour
40 %

@Temperature 150 °C,
Time 3600 sec
40 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 120 °C
0.0833 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 20
T10 (302°F, ODR)
29
T90 (302°F, ODR)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved