Polymer Property : Linear Mold Shrinkage = 0.032 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.032 cm/cm
0.032 in/in
4.0 inch Disk; ASTM D955
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
Linear Mold Shrinkage 0.032 cm/cm
0.032 in/in
Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber
20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.