Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
DIN 53479
Linear Mold Shrinkage 0.032 cm/cm
0.032 in/in
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Tensile Modulus 4.80 GPa
696 ksi
ASTM-D790
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM-D790
Izod Impact, Notched 0.950 J/cm

@Temperature 23.0 °C
1.78 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
140 °C
284 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in