Physical Properties Metric English Comments
Linear Mold Shrinkage 0.025 - 0.035 cm/cm
0.025 - 0.035 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Linear Mold Shrinkage 0.025 - 0.035 cm/cm
0.025 - 0.035 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
Linear Mold Shrinkage 0.025 - 0.035 cm/cm
0.025 - 0.035 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Linear Mold Shrinkage 0.025 - 0.035 cm/cm
0.025 - 0.035 in/in
ISO 294-4
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound
PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o..
Linear Mold Shrinkage 0.00 - 0.035 cm/cm
0.00 - 0.035 in/in
ASTM 1917
Nitriflex SB-1009 Styrene Butadiene Copolymer
Applications: Used to promote better dimensional stability in articles like profiles, hoses, shoe sole and also recommended to PSA adhesives and adhesives for vertical applications. Available in bal..
Linear Mold Shrinkage 0.0025 - 0.035 cm/cm
0.0025 - 0.035 in/in
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound
BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts...