Polymer Property : Linear Mold Shrinkage, Flow = 0.00080 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00080 - 0.0010 cm/cm

@Time 86400 sec
0.00080 - 0.0010 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.00080 - 0.0018 cm/cm

@Thickness 3.20 mm
0.00080 - 0.0018 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East)
PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays.
Linear Mold Shrinkage, Flow 0.00080 - 0.0028 cm/cm

@Time 86400 sec
0.00080 - 0.0028 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.00080 - 0.0010 cm/cm

@Time 86400 sec
0.00080 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow >= 0.00080 cm/cm
>= 0.00080 in/in
on Tensile Bar; E2P method
Eurostar Staramide ACF6 PA66, 30% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF6 is a 30% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.