Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0020 - 0.0028 cm/cm

@Time 86400 sec
0.0020 - 0.0028 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP LX08411 PEEK
LNP* THERMOCOMP* LX08411 is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added feature of this material is: Opaque.
Linear Mold Shrinkage, Flow 0.00080 - 0.0028 cm/cm

@Time 86400 sec
0.00080 - 0.0028 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0023 - 0.0028 cm/cm

@Thickness 3.20 mm
0.0023 - 0.0028 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..