Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0043 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0043 - 0.0047 cm/cm

@Thickness 3.20 mm
0.0043 - 0.0047 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Linear Mold Shrinkage, Flow 0.0043 - 0.0047 cm/cm

@Thickness 3.20 mm
0.0043 - 0.0047 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Linear Mold Shrinkage, Flow 0.0043 cm/cm
0.0043 in/in
ISO 294-4, 2577
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow)
Linear Mold Shrinkage, Flow 0.0043 cm/cm

@Time 86400 sec
0.0043 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber.
Linear Mold Shrinkage, Flow 0.0043 cm/cm
0.0043 in/in
60x60x2mm; ISO 294
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Linear Mold Shrinkage, Flow 0.0043 cm/cm
0.0043 in/in
60x60x2mm; ISO 294
BASF Ultradur S 4090 G4 20% Glass Filled PBT
Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio..
Linear Mold Shrinkage, Flow 0.0043 cm/cm
0.0043 in/in
ISO 2577
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..
Copyright © lookpolymers.com All Rights Reserved