Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0050 - 0.0051 cm/cm @Time 86400 sec |
0.0050 - 0.0051 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |