Polymer Property : Linear Mold Shrinkage, Flow = 0.0054 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0054 cm/cm
0.0054 in/in
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY
Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe..
Linear Mold Shrinkage, Flow 0.0054 cm/cm
0.0054 in/in
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY
Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a..
Linear Mold Shrinkage, Flow 0.0054 cm/cm
0.0054 in/in
60x60x2 mm; ISO 294
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..