Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applications: TECHNYLSTAR TM S 218 MZ20 V10 BLACK 2N is suitable for applications where a compromise of rigidity and dimensional stability is required, as engine cover. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183/A
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0054 cm/cm
0.0054 in/in
Linear Mold Shrinkage, Transverse 0.0108 cm/cm
0.0108 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 2.8 %
2.8 %
ISO 527 Type 1A
Tensile Modulus 7.80 GPa
1130 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 3.70 kJ/m²
1.76 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.340 J/cm²
1.62 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 220 - 230 °C
428 - 446 °F
Front Barrel Temperature 245 - 250 °C
473 - 482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Compression Zone 245-250°C