Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00700 cm/cm

@Thickness 3.17 mm
0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers Polysulfone PSF P170-64170 White PSU
Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio..
Linear Mold Shrinkage, Flow 0.00700 - 0.0100 cm/cm
0.00700 - 0.0100 in/in
Injection; ISO 2577
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..