Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.011 - 0.0114 cm/cm
0.011 - 0.0114 in/in
ISO DIS 294-4
Wellman EcoLon® MRGF1619-BK3 19% Mineral/Glass Reinforced Post Consumer Compound Nylon 66
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman.