Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm @Thickness 3.17 mm |
0.011 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0615 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.019 cm/cm | 0.011 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | ASTM D955 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.019 cm/cm | 0.011 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | 60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
LATI Latistat 47/7-03 PP Copolymer Dissipative product based on Polypropylene copolymer (PPc). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP HAL23 PA11 (Europe-Africa-Middle East) LNP* LUBRICOMP* HAL23 is a compound based on PA 11 resin containing Aramid Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.016 cm/cm | 0.011 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East) LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Treatment Temp. 130 °C, Time 3600 sec |
0.011 - 0.015 in/in @Treatment Temp. 266 °F, Time 1.00 hour |
annealed; ASTM D 955 |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
|
Unitika A1025NO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6 Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-BK11 Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |