Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.019 - 0.026 cm/cm
0.019 - 0.026 in/in
ASTM D955
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
60x60x2 mm; ISO 294-4
Gromax ATE70-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 230 PA66, DRY
Description: Unreinforced and modified polyamide 66, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 230 offers excel..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PP 0096 S LE Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 216 PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PA6 FR 544
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedRoHS Compliance: RoHS CompliantInformation provided by TP Com..
Linear Mold Shrinkage, Flow 0.019 - 0.024 cm/cm

@Thickness 3.20 mm
0.019 - 0.024 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® FXV310SK PBT
VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances.
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® LDPE 0098 S LE
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 208KBK-10N-L PA66, DRY
Description: Polyamide 66, highly UV-resistance, toughness modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL A 208K BK 10N-L is used in all sectors of industry, ..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
24 hours + 30 min at 93°C
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ISO DIS 294-4
Wellman Wellamid® XT1606-N Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Linear Mold Shrinkage, Flow 0.019 - 0.021 cm/cm

@Time 86400 sec
0.019 - 0.021 in/in

@Time 24.0 hour
ISO 294
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded
Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Eurotec
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 75 A.1 black TPE-S, Shore A75, black
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 2577
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona..