Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0392 cm/cm

@Thickness 3.17 mm
0.0392 in/in

@Thickness 0.125 in
ASTM D955
Network Polymers Softflex® 3300
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.