Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 50.8 cm @Pressure 27.6 MPa, Temperature 163 °C |
20.0 in @Pressure 4000 psi, Temperature 325 °F |
Mesa |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Spiral Flow | 50.8 cm | 20.0 in | NOVA Chemicals snake flow number |
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |