Physical Properties Metric English Comments
Spiral Flow 30.0 - 70.0 cm
11.8 - 27.6 in
Average value: 47.7 cm Grade Count:6
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..