Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 45.0 cm @Temperature 220 °C |
17.7 in @Temperature 428 °F |
ASTM D3123 |
Total PSI 8350 (AS) High Impact Polystyrene Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st.. |
|||
Spiral Flow | 45.0 cm | 17.7 in | AKRO |
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Spiral Flow | 45.0 cm | 17.7 in | AKRO |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |