Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 55.0 cm @Temperature 220 °C |
21.7 in @Temperature 428 °F |
ASTM D3123 |
Total PS CPDS 822 Standard Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 822 is a good flow, environmentally friendly high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good d.. |
|||
Spiral Flow | 55.0 - 65.0 cm | 21.7 - 25.6 in | Average value: 60.7 cm Grade Count:6 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Spiral Flow | 55.0 - 100 cm | 21.7 - 39.4 in | Average value: 82.4 cm Grade Count:16 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |