Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 61.0 cm
24.0 in
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 61.0 cm
24.0 in
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Spiral Flow 61.0 cm
24.0 in
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Spiral Flow 61.0 cm
24.0 in
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 61.0 cm

@Thickness 2.50 mm
24.0 in

@Thickness 0.0984 in
at 254°C melt temp.
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Spiral Flow 61.0 cm

@Thickness 2.50 mm
24.0 in

@Thickness 0.0984 in
at 254°C melt temp.
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Spiral Flow 61.0 cm

@Thickness 2.50 mm
24.0 in

@Thickness 0.0984 in
at 254°C melt temp.
Covestro Bayblend® T 45 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
Spiral Flow 61.0 cm
24.0 in
Cross Section: 7[mm]x3.5[mm]; AKRO
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Spiral Flow 61.0 cm

@Thickness 2.50 mm
24.0 in

@Thickness 0.0984 in
at 254°C melt temp.
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend  (discontinued **)
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin..