Polymer Property : Brookfield Viscosity = 2200 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 2200 cP

@Temperature 25.0 °C
2200 cP

@Temperature 77.0 °F
in Toluene, 37.5% solids
Lucite International Elvacite ® 2550 Acrylic Resin
Elvacite® 2550 is a solid bead methacrylate copolymer resin. It is designed to provide excellent adhesion to metal surfaces and is a resin with good flexibility and medium molecular weight. As su..